Where can I see pictures? of the fire steels?
Rowland of Roseburg, OR 97470
10 miles to the nearest Red Light
There is a very fine line between
"hobby" and "mental illness
----- Original Message ----- 
From: "Daniel Kretchmar" <dan at irontreeworks.com>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Thursday, February 16, 2006 6:18 PM
Subject: Re: [TheForge] fire steel materials


> My fire steels are made from 1/2 strips cut from an old industrial planer 
> blade.  They are 1/4 inch thick and according to the steel yard where I 
> bought the old blade, it is 1095.  I tried lots of other metals AR232, old 
> files, old coil springs, drill rod, etc, and the planer blade consistantly 
> makes the sparkiest steels
>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
> 



More information about the TheForge mailing list