[TheForge] Chip Bed Forge

Michael Horgan lughaid at earthlink.net
Thu Feb 16 22:48:10 EST 2006


I'll be using alumina pebbles from 
http://www.richwoodindustries.com/nuggets.html  which were 
recommended for forge use by one of their engineers. Paul Boulay is 
kindly splitting a 50 pound box with me.

I'll be interested too, Rick. ;^)

At 08:56 AM 2/16/2006, you wrote:
>Michael,
>I contacted one of the English Mfgrs last summer.  They do not make an
>export version because of electric power standards compatibility.  They
>would ship/sell the ceramic media.  I did not pursue this further.
>
>Where are you getting the media?
>
>I am very interested in your experience with this combustion approach.
>
>-Rick

Michael D. Horgan , lughaid at earthlink.net
http://members.aol.com/lughaid/
posting from
  A BRAZEN FORGERY
Blacksmithing and Metalwork
Claremont, Ca.




More information about the TheForge mailing list