[TheForge] Cast Iron

Ralph Sproul brhlbsmt at mcttelecom.com
Wed Feb 15 11:54:28 EST 2006


	If you use a needle scaler on lead paint - don't forget the resperator!!!
Lead paint mushes, smears, and makes a lot of dust with the parts that
aren't chipping right off.

Ralph

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net]On Behalf Of Rowland Smuck
Sent: Wednesday, February 15, 2006 11:19 AM
To: Sponsored by ABANA
Subject: Re: [TheForge] Cast Iron


Rick use a needle scaler, they are cheap from Harbor Freight.
Rowland of Roseburg, OR 97470
10 miles to the nearest Red Light
There is a very fine line between
"hobby" and "mental illness
----- Original Message -----
From: "Rick" <rick at smokyforge.com>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Tuesday, February 14, 2006 3:57 PM
Subject: Re: [TheForge] Cast Iron


> Hello again -
>
>    Thanks for all the reply's on the cast iron cleaning.  I hadn't thought
> about needing to breathe while the lead based paint is burning in the
> shop. Already have enough sinus and breathing problems without adding to
> them.  I guess I'll just stick to the putty knife and degreaser.
>
> Thanks again,
> Rick
>
>
>> Hi Guys -
>>
>>    I am not someone who knows much about cast iron.  I have an old
>> power
>> hack saw that I am cleaning and trying to resurrect.  It is under
>> layersw of
>> grease and even more layers of paint.  What I need to know is, will it
>> hurt
>> cast iron to go into the forge fire for a while to burn off some of this
>>
>> crap?  I would save LOTS of time and trouble if I could burn it off
>> without
>> damaging the parts.  Has anyone done this successfully, or does someone
>> know
>> that it shouldn't be done?
>>
>
>
>
> --
> No virus found in this outgoing message.
> Checked by AVG Free Edition.
> Version: 7.1.375 / Virus Database: 267.15.5/256 - Release Date: 2/10/2006
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>

_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________






More information about the TheForge mailing list