Mike Porter wrote: > Beyond the iron oxide, IR suppression is tied to > the filter's darkness. Just get gold coated optics. Gold filters 99% IR. Glass Schell makes gold-flashed didymium glasses and full face shields. I know they're still in business, but their site seems to have gone into hiding. -Andy