What about silver brazing it?? That works slick.........

Ray

---- Rick Korinek <rickkorinek at verizon.net> wrote: 
> I have a related question regarding bronze.  I have an upcoming project to
> make fireplace doors out of bronze.  I would like to fasten the back screen
> frames to the door frames without fasteners like rivet heads showing on the
> front surfaces.  Is it possible to fasten threaded studs to the bronze by
> welding?  Something like 1/4"-20 or #10.  The stud material is not
> important--could be steel, bronze or brass, whatever will adhere nicely.
> 
> I have the equipment to TIG, Mig and torch weld.  What would you recommend?
> -Rick
> 
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Bill Roberts
> Sent: Thursday, February 02, 2006 9:05 AM
> To: Sponsored by ABANA
> Subject: Re: [TheForge] Forging Bronze
> 
> Hi David,
> I've always used mig or tig. You can get spools of silicon bronze  
> wire, and silicon bronze tig rod. Gives a better color match, when  
> it's time for the patina. FWIW.
> 
> Bill Roberts
> www.CustomDesignMetalArts.com
> 
> 
> 
> On Feb 2, 2006, at 9:09 AM, Hufford, David wrote:
> > Bill:
> > Speaking of silicon bronze ... how about welding?  Can it be welded  
> > using oxy-acetylene with bronze brazing rod?  If so, any  
> > pointers ... ?
> > David Hufford
> >
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 
> 
> 
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 



More information about the TheForge mailing list