[TheForge] Re: 2 Questions
Rick Korinek
rickkorinek at verizon.net
Wed Feb 1 20:57:30 EST 2006
George,
I assume you were working the lengths hot. What kind of forge and how did
you get pieces from forge to hammer?
-Rick
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of george rousis
Sent: Tuesday, January 31, 2006 6:09 PM
To: Sponsored by ABANA
Subject: Re: [TheForge] Re: 2 Questions
i was just making some octagon bar the other day and threw together a stand
with a piece of 3"o.d. pipe 3' long at the aproximate hieght of the hammer
and it worked fine. iwas working 7' to10"ers 3/4 - 1" square
----- Original Message -----
From: "Rick Korinek" <rickkorinek at verizon.net>
To: "'Sponsored by ABANA'" <theforge at mailman.qth.net>
Sent: Monday, January 30, 2006 7:52 AM
Subject: RE: [TheForge] Re: 2 Questions
> Thanks to those who offered suggestions on how to handle long stock. The
> idea of in- and-out feed supports for the power hammer, forge and anvil
make
> sense. I like the idea of positioning the anvil in-line to facilitate
> straightening and Mike's idea for a rotating stock support is innovative,
> but I thing getting a long piece into the chain loop might be a hasstle.
>
> One area I am still puzzling over is heating the stock. Without a
conveyor
> table set up, I think getting stock in and out of a gas forge would be
real
> hard on the forge. But perhaps this is the way to go--put every thing in
> line: forge, power hammer, anvil and hossfeld. Then put some guides in
and
> out of the forge to keep the stock away from the refractory. Right now, I
> would probably use the coal forge because it is open.
>
> -Rick
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list