On Feb 1, 2006, at 8:28 AM, Ron Swisher wrote:
> Does anyone on the list own a 75 lb. Bull? I have recently noticed a
> decrease in the bpm and an inability to get an air cushion at the top
> of the stroke. I have readjusted the valves in accordance with the
> tape sent out by Tom Tro... entitled "Bull 75B" but this has not
> helped. I shot an email to Tom via his Phoenix Hammer web site but no
> response. Any thoughts? Anyone experience similar problems?
>
> Ron
>
_______
Have you taken the air cylinder apart? Could be the rubber "rings" are
worn or maybe a piece of dirt is making the rings leak.
Bob