[TheForge] RE: Tool Steel

Chuck Robinson robi5515 at bellsouth.net
Sat Dec 23 14:31:08 EST 2006


Thanks everyone for your recommendations i'm checking them all out.
Chuck
----- Original Message ----- 
From: "Bob Ehrenberger" <eforge at centurytel.net>
To: "theforge" <theforge at mailman.qth.net>
Sent: Friday, December 22, 2006 7:54 AM
Subject: [TheForge] RE: Tool Steel


> Chuck,
>
> We get our tool steel from Admeral Steel in Chicago.
> They will work with you and don't mind small orders.
>
> Robert Ehrenberger
> Shelbyville, Mo.
> eforge at centurytel.net
>
> ----Original Message----
> Date: Thu, 21 Dec 2006 10:47:15 -0600
> From: "Chuck Robinson" <robi5515 at bellsouth.net>
> Subject: [TheForge] Tool steel source
>
> I need a source or sources for round and square stock  W-1 and H-13 in 
> small
> quantities. The GCBA conference in February is featuring Frank Turley as 
> the
> main demonstrator and he requires them for his demo.
> Chuck
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
> 



More information about the TheForge mailing list