some cold forging aluminum here.
http://www.youtube.com/watch?v=Zdi6C-oADEI
_________________
On Dec 19, 2006, at 8:11 PM, Barking Crow wrote:
> I've been playing around with forging some trashpile aluminum rods
> about 3/8 ". I forge it cold until I think it may break then stop and
> heat it with my little mapp gas torch until I think it might be
> annealed and then let it cool and start again. Having fun punched and
> drifted a nice little hole. I started out to make a wedge of aluminum
> to put in a collection of wedges of different size, shape, and
> material that I plan to give my daughter's boyfriend as a gift. Then
> I was having fun and kept on playing for awhile. My question is how
> hot do I have to get the aluminum (a guess since I don't really know
> what the alloy is) before letting it cool? I've been heating the
> piece until it is just barely red in the dark. Is there a better way?
>
> Thanks, Jeff in Tallahassee
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list