Pete: I doubt that a forge weld is enhanced by the presence of any foreign
material, except in that material's capacity to act as an oxygen barrier (a
la flux). I have no solid proof, one way or the other, however. Grant
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net]On Behalf Of Peter Fels And
Phoebe Palmer
Sent: Friday, December 15, 2006 11:02 PM
To: mspencer at tallships.ca; Sponsored by ABANA
Subject: [TheForge] I don't get it...
How come a forgeweld is enhanced by the presence of oil (
supposed to consume the oxy)...
BUT
A mere hint of the memory of grease ruins a TIG weld?
Would one of you adults please esplane ta me?...pete f
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
--
No virus found in this incoming message.
Checked by AVG Free Edition.
Version: 7.1.409 / Virus Database: 268.15.21/589 - Release Date: 12/15/2006
More information about the TheForge
mailing list