OK back to the video... a few things... surely it's the boss wearing
the clean white shirt and waving his hat about like a lunatic... he
looks pretty peeved right at the beginning.

A question.. can anyone tell me what it is they are throwing at the
big chunk of hot steel? Is it some form of BORAX or even sand to keep
the scaling down? if it is it't not very effective! scale just pours
off that thing everytime it gets whacked!

Also why do you think they are using those large cutting blades? Does
anyone have a clue about this video and if there is any more footage?
I'd love to see more of it.

stephen

On 12/12/06, Hufford, David <David.Hufford at eku.edu> wrote:
> The slide rule ... what an ingenious implement.  I used one all through
> college.  Wish I still had it.  Not long ago I saw one in an 'antique'
> shop, along side an IBM PCJr.
> David Hufford
> Richmond KY
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
>


-- 
Come and visit me in cyberspace..
http://wombatforge.googlepages.com/
http://wombatforge.blogspot.com/


More information about the TheForge mailing list