[TheForge] Rivet Set

Dan Tull dantull at numail.org
Wed Aug 30 15:19:57 EDT 2006


Now you are thinking like a blacksmith.
Drill a little dimple first as the bearing isn't going to stay there long.
Might as well use three or four popular sizes while you're at it.

----- Original Message ----- 
From: "Jeffrey Polaski" <jeff.polaski at rgs.uci.edu>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Wednesday, August 30, 2006 2:24 PM
Subject: RE: [TheForge] Rivet Set


Thanks for the advice. I'll make one by pounding a ball bearing or maybe
a rivet head into a piece of hot metal.



Jeff Polaski
Research and Graduate Studies Webmaster
University of California, Irvine
http://www.rgs.uci.edu/
949.824.6363

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Jeffrey Polaski
Sent: Tuesday, August 29, 2006 3:50 PM
To: Sponsored by ABANA
Subject: [TheForge] Rivet Set

I have a few knives that I'd like to finish and I'd like to use some
round-head or truss-head rivets to attach the handles to the blades.
I'll probably use 1/8" or 3/16" rivets. 

Does any one know here to get a rivet set for round or truss-head
rivets? 


Jeff Polaski
Research and Graduate Studies Webmaster
University of California, Irvine
http://www.rgs.uci.edu/
949.824.6363


_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________



_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________






More information about the TheForge mailing list