[TheForge] Making a Shovel
Jeffrey Polaski
jeff.polaski at rgs.uci.edu
Mon Aug 28 18:01:07 EDT 2006
> put it in the fire and hammer till it looks like the 1860's.
You should but that in your sig!
Jeff Polaski
Research and Graduate Studies Webmaster
University of California, Irvine
http://www.rgs.uci.edu/
949.824.6363
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Chris Worsley
Sent: Monday, August 28, 2006 1:43 PM
To: Bob Ehrenberger; Sponsored by ABANA
Subject: Re: [TheForge] Making a Shovel
How important is this? Is the shovel going into a museum, or perhaps a
historical site where someone will lecture on the making of Civil War
shovels in detail?
One thing you could do is try to get the seller of the shovel on ebay to
send you a picture of the back of the blade. He has no buyers as of now
and might do it if you sound interested.
Otherwise I would just forge weld a socket on the back and rivit the
handle in place.
If forge welding thin stock is a problem, mig it, put it in the fire and
hammer till it looks like the 1860's.
Chris
Bob Ehrenberger wrote:
>Chris,
>
>Thanks for the link. The problem is that this picture, like most
pictures
>I've located, doesn't show the critical part of the shovel, ie: how is
the
>handle attached. This one shows that there is some sort of a socket
for
>the handle but was the socket forged from the same piece of steel that
the
>blade was or was it welded on? Is there a support on the back side?
Most
>modern shovels seem to have a plate spot welded to the back to help
support
>the handle.
>
>Robert Ehrenberger
>Shelbyville, Mo.
>eforge at centurytel.net
>
>----Original Message----
>Date: Sun, 27 Aug 2006 10:58:43 -0700
>From: Chris Worsley <cpworsley at cox.net>
>Subject: Re: [TheForge] Making a Shovel
>
>Here is one on ebay:
>http://cgi.ebay.com/Civil-War-Period-D-Handle-Shovel_W0QQitemZ130019996
929QQcmdZViewItem
>
>If you are looking for a fireplace shovel, look in Sonn's book Early
>American Wrought Iron.
>
>Google 'civil war shovel' under Images and get another picture.
>Instructions: Make it look just like the pictures.
>
>Chris
>
>
>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list