[TheForge] Soldering Stainless- or welding
Woolley
wjec at verizon.net
Thu Aug 24 10:05:18 EDT 2006
Ron,
I lit up with the tig and promptly burned up my 3/32, not good since I will
have to weld 60 or more pieces that have been coiled into a little spiral
before being attached. Didn't try o/a.
Bill
----- Original Message -----
From: "Ron Childers" <munlaw2 at hcsmail.com>
To: "'Sponsored by ABANA'" <theforge at mailman.qth.net>
Sent: Wednesday, August 23, 2006 1:17 PM
Subject: RE: [TheForge] Soldering Stainless- or welding
I've had good luck just welding with ss rod, arc, tig or o/a. No color
variation when polished.
Ron C
move to I-use a file a file her a file your view a man they a man file for
you to a file a home for a a a home they were home man they say a a file a a
a view to you this man-a file a may file a have a file they may have they
say this new one new home a file a new home a-a a a mass may know a home the
a matter I-C.-to the move a
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Woolley
Sent: Wednesday, August 23, 2006 11:31 AM
To: Sponsored by ABANA
Subject: Re: [TheForge] Soldering Stainless
Thanks Dan
----- Original Message -----
From: "Dan Brewer" <danqualman at gmail.com>
To: "'Sponsored by ABANA'" <theforge at mailman.qth.net>
Sent: Tuesday, August 22, 2006 11:40 PM
Subject: RE: [TheForge] Soldering Stainless
> Then silver solder /silver braze is what you want. The silver is the
> wetting agent in the filler rod. Just tell the nice folk at the welding
> store what you are looking for. If you do a scarf joint it will be just
> about as strong as you can do with the rod.
>
> Dan in Auburn
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Woolley
> Sent: Tuesday, August 22, 2006 8:34 PM
> To: Sponsored by ABANA
> Subject: Re: [TheForge] Soldering Stainless
>
> Dan,
>
> Of all things, I'm making a cupcake tree for a pastry chef to be used in
> a
> restaurant (several if I get this prototype right) The 1/8 rod will be
> the
> spike and the 3/32 will be a little flattened spiral joined to the spike
> for
>
> the cupcake to rest on.
>
> Bill
>
> ----- Original Message -----
> From: "Dan Brewer" <danqualman at gmail.com>
> To: "'Sponsored by ABANA'" <theforge at mailman.qth.net>
> Sent: Tuesday, August 22, 2006 10:09 PM
> Subject: RE: [TheForge] Soldering Stainless
>
>
>> Why are you trying to join the pieces together?
>>
>> Dan in Auburn
>>
>> -----Original Message-----
>> From: theforge-bounces at mailman.qth.net
>> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Woolley
>> Sent: Tuesday, August 22, 2006 7:01 PM
>> To: theforge at mailman.qth.net
>> Subject: [TheForge] Soldering Stainless
>>
>> Greetings,
>>
>> I know this has probably been discussed here before but I need to know
>> what
>> material to use to join 2 pieces of 316L or 308 ss tig rod together, 1/8
>> and
>> 3/32. Silver solder? I obviously need to keep the heat down so I won't
>> burn up the rod. Thanks for any help.
>>
>> Regards,
>> Bill Woolley
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> password: anvil
>> ___________
>>
>>
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> password: anvil
>> ___________
>>
>>
>>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list