[TheForge] Soldering Stainless- or welding
James Binnion
jbin at well.com
Thu Aug 24 01:33:21 EDT 2006
On Aug 23, 2006, at 12:13 PM, Michael wrote:
> just like the
> so-called silver solder sold by jewelers supply outfits are nothing
> more
> than short lengths of standard silver braze wire, snipped from
> standard
> reasonably priced spools, and then sold in plastic baggies-for
> outrageous
> prices. Drug dealers have nothing on these guys, and it's all legal
> to boot!
>
> Mikey
Mikey,
You must be buying at the wrong places I buy silver solder from
jewelers suppliers at better prices than from the welding suppliers.
James Binnion
jbin at well.com