Since the subject is at hand I would like to relate an experience from today
and perhaps someone might conjecture an opinion.
I needed to solder a stainless handle to a stainless bowl. I was using easy
silver. I first tried my general use flux which is Stay Clean from Harris. I
use this with all lead solder and find it excellent. The silver balled up and
did not flow. Next I tried Rio Grande Rio Ready Flux for Silver and Gold.
Again it balled up and did not flow. Last I tried Ultra Flux Silver Brazing Flux
from Wolverine and it flowed quickly and nicely and is a solid joint.
Is there that much difference in fluxes or do you think I was doing
something else wrong...like applying too much heat too fast or whatever. I have a
bunch more of these to go so welcome any opinions.
Kindest thanks
Don Plummer