[TheForge] Soldering Stainless
Dan Brewer
danqualman at gmail.com
Tue Aug 22 23:40:44 EDT 2006
Then silver solder /silver braze is what you want. The silver is the
wetting agent in the filler rod. Just tell the nice folk at the welding
store what you are looking for. If you do a scarf joint it will be just
about as strong as you can do with the rod.
Dan in Auburn
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Woolley
Sent: Tuesday, August 22, 2006 8:34 PM
To: Sponsored by ABANA
Subject: Re: [TheForge] Soldering Stainless
Dan,
Of all things, I'm making a cupcake tree for a pastry chef to be used in a
restaurant (several if I get this prototype right) The 1/8 rod will be the
spike and the 3/32 will be a little flattened spiral joined to the spike for
the cupcake to rest on.
Bill
----- Original Message -----
From: "Dan Brewer" <danqualman at gmail.com>
To: "'Sponsored by ABANA'" <theforge at mailman.qth.net>
Sent: Tuesday, August 22, 2006 10:09 PM
Subject: RE: [TheForge] Soldering Stainless
> Why are you trying to join the pieces together?
>
> Dan in Auburn
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Woolley
> Sent: Tuesday, August 22, 2006 7:01 PM
> To: theforge at mailman.qth.net
> Subject: [TheForge] Soldering Stainless
>
> Greetings,
>
> I know this has probably been discussed here before but I need to know
> what
> material to use to join 2 pieces of 316L or 308 ss tig rod together, 1/8
> and
> 3/32. Silver solder? I obviously need to keep the heat down so I won't
> burn up the rod. Thanks for any help.
>
> Regards,
> Bill Woolley
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list