[TheForge] Soldering Stainless

Woolley wjec at verizon.net
Tue Aug 22 22:01:23 EDT 2006


Greetings,

I know this has probably been discussed here before but I need to know what material to use to join 2 pieces of 316L or 308 ss tig rod together, 1/8 and 3/32.  Silver solder?  I obviously need to keep the heat down so I won't burn up the rod. Thanks for any help.

Regards,
Bill Woolley