[TheForge] RE: Casting; to be or not to be...
Washington, Aubrey O.
awashington at ou.edu
Wed Aug 2 15:42:18 EDT 2006
Okay. I'll try the acid test. AND, I'll be sure my son is very careful about breathing fumes.
________________________________
From: theforge-bounces at mailman.qth.net on behalf of Bruce Freeman
Sent: Wed 8/2/2006 2:37 PM
To: theforge at mailman.qth.net
Subject: RE: [TheForge] RE: Casting; to be or not to be...
Ask the late Paw Paw Wilson how dangerous "brass fumes' (i.e., zinc
fumes) are: http://www.anvilfire.com/iForge/
He was exposed in an indoors environment. Outdoors would help a lot,
but the key is not to breathe the stuff.
Pickle an ingot in acid (or put a drop of acid on the ingot). If the
color changes from "gold" to copper, then it's probably zinc - you've
etched the zinc out of the surface.
Bruce
NJ