I have two types of anvils; ones that are steel and ones that are cast iron.
The steel ones ring like a bell, so to speak and the iron ones don't. The
cast iron ones that are gray iron all the way through, i.e., cheap, are dead
and lifeless. I have one with a chilled face that is harder than any of my
steel anvils and has an excellent rebound even though it goes thud when you
hit it. Striking on the horn does make a feeble ring.
They all have their own personalities.