[TheForge] Drilling hard metal-Thanks!

robert hensarling rhrocker at hilconet.com
Sat Apr 22 00:04:46 EDT 2006


Ok, Good, thanks Grant.  I'll check into it all on Monday.
Robert
----- Original Message ----- 
From: "Grant Marcoux" <gblacksmith at alamedanet.net>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Friday, April 21, 2006 10:47 PM
Subject: RE: [TheForge] Drilling hard metal-Thanks!


> Robert:  I get mine, in drill rod form, from Summerville Steel 
> Corporation.
> They have a will-call office in San Leandro, CA.    They are in Kent, WA 
> and
> can probably drop-ship to you.  Call them at 1-800-552-5030.  Admiral 
> still
> offers ok prices for small quantity, but maybe Summerville can beat it.
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net]On Behalf Of robert hensarling
> Sent: Friday, April 21, 2006 11:03 AM
> To: Sponsored by ABANA
> Subject: Re: [TheForge] Drilling hard metal-Thanks!
>
>
> Grant, what's a good current source for L-6.  I've purchased it before 
> from
> Admiral, but maybe there's another good place to buy it.
> Robert
>
> ----- Original Message -----
> From: "Grant Marcoux" <gblacksmith at alamedanet.net>
> To: "Sponsored by ABANA" <theforge at mailman.qth.net>
> Sent: Friday, April 21, 2006 12:56 PM
> Subject: RE: [TheForge] Drilling hard metal-Thanks!
>
>
>> Andy:  L-6 is one of my fave plain steels for blades....great toughness
>> (nickel) and ease of sharpening.  Some folks are making excellent sword
>> blades, both cutters and thrusters, from this steel.  Sadly, I'm not
>> convinced that it will be around much longer.  Maybe some others can 
>> weigh
>> in on this.
>>
>> Yes, make the cooling as slow as possible.  When I was first taught to
>> forge
>> blades, my first forged knife was of 5/8" L-6 drill rod.  We annealed it
>> under the forge ashes, on the highly heated brick hearth.  The blade was
>> softened to the point that it would be cut readily with a file.  If this
>> is
>> the case, it will readily drill with a sharp HSS bit. Don't forget to
>> pilot
>> hole and to pickle the scale off.  Grant
>>
>> -----Original Message-----
>> From: theforge-bounces at mailman.qth.net
>> [mailto:theforge-bounces at mailman.qth.net]On Behalf Of Gladish Family
>> Sent: Friday, April 21, 2006 8:28 AM
>> To: Sponsored by ABANA
>> Subject: Re: [TheForge] Drilling hard metal-Thanks!
>>
>>
>> Thanks for the input, everyone!
>> A light went on when it was said that L6 is slightly air-hardening: I
>> think I simply have to take the Slow Cooling part of this much more
>> seriously.
>>
>> Andy Gladish
>>
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login:  blacksmithblacksmith at hotmail.com
>> password:  anvil
>> ___________
>>
>>
>>
>>
>> --
>> No virus found in this incoming message.
>> Checked by AVG Free Edition.
>> Version: 7.1.385 / Virus Database: 268.4.5/321 - Release Date: 4/21/2006
>>
>>
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login:  blacksmithblacksmith at hotmail.com
>> password:  anvil
>> ___________
>>
>>
>>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
>
>
> --
> No virus found in this incoming message.
> Checked by AVG Free Edition.
> Version: 7.1.385 / Virus Database: 268.4.5/321 - Release Date: 4/21/2006
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
> 




More information about the TheForge mailing list