[TheForge] Finally I can upload something worthwhile.
Ralph Sproul
brhlbsmt at mcttelecom.com
Sat Apr 8 07:54:07 EDT 2006
Been a long week........I meant oven opening ......... Right of the hood -
not left.
Will you be making a door for the oven opening - or is it like a "left open"
warming oven? At any
rate - really nice masonry work.
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net]On Behalf Of Ralph Sproul
Sent: Saturday, April 08, 2006 7:34 AM
To: Sponsored by ABANA
Subject: RE: [TheForge] Finally I can upload something worthwhile.
Nice job on the hood Stephen, Is the large masonry wall part of an in house
heater and this end is the kitchen with your range hood and the oven to the
left?
Ralph
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net]On Behalf Of Stephen Viola
Sent: Friday, April 07, 2006 3:28 PM
To: The Forge
Subject: [TheForge] Finally I can upload something worthwhile.
Hi all,
I have just uploaded 4 images of the most recent project COMPLETED!!!!
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
look in the "new images of recent works" folder.
copper 030
copper 058
copper 067
copper 054
The best thing about this project was that there was very little
bought ready made.
2 copper sheets 1m x 2m, some 3 mill copper wire and ready made copper
rivets. Well the rivets needed a lot of work but they were bought. I
should mention the light and filter box were also bought.. but again
modified.
But pretty much everything else was cut / machined / bent and forged into
shape.
This copper hood is the end result!!
Wombat
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list