[TheForge] charcoal
Jerry Smith
jerry_smith at anvilsandinkstudios.com
Sun Apr 2 17:25:36 EDT 2006
I would like to know, I am in Eastern Ohio in a town
called Somerton, we are 20 miles south from BFE Ohio.
Jerry
--- Bob Willman <blcksmth at wcnet.org> wrote:
> I don't know where you are located, but we are
> having a charcoal
> making demonstration at our 20th annual Hammer-In
> May 5-6-7 near Defiance,
> Ohio. I am looking forward to it. If any are
> interested in attending let me
> know.
>
>
> Bob Willman
> Bowling Green, Ohio
> The Eagle's Anvil
> WB8NQW
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf
> Of Bob Smolen
> Sent: Sunday, April 02, 2006 3:41 AM
> To: Sponsored by ABANA
> Subject: [TheForge] charcoal
>
> I have some cull logs and wondered if anyone has
> tried making charcoal and
> is it worth the effort? I use gas and also like coal
> but it would be nice to
> make own fuel if practical. There are a lot of
> sawmills in the area and I
> can get trimmings cheaply, but is there a lot of
> work once you have the
> wood?
> Thanks,
> Bob
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list