I made mine out of the 18g doors from a datacenter air conditioning
unit, lined it with 3" 2500 deg refractory brick and high temp mortar.
Doors are castable, 2" think. Fired by a mankel 3-burner and a blower.
The thing weighs about 300 pounds.
It works well, but it's not how I'd do it again.
J
--- Grover Richardson <grover.richardson at gtri.gatech.edu> wrote:
> I make mine out of 8 pound kaowool, surrounded by air conditioning
> duct.
> Sheet metal screws hold it together. For travelling, I place it in a
> 5
> gallon sheetrock mud bucket.
>
> >*>-----Original Message-----
> >*>From: theforge-bounces at mailman.qth.net
> >*>[mailto:theforge-bounces at mailman.qth.net] On Behalf Of
> >*>Steven.Walker at its.state.ms.us
> >*>Sent: Tuesday, September 27, 2005 12:01 PM
> >*>To: theforge at mailman.qth.net
> >*>Subject: Fw: [TheForge] Gas forge Question
> >*>
> >*>
> >*>
> >*>>I'd like to point out that we often like to overbuild stuff,
> forges
> >*>>being
> >*>no
> >*>>exception.
> >*>
> >*>That's another reason I built mine with a freon tank instead
> >*>of a propane tank.....the freon tank I had was much lighter
> >*>a propane tank because it's constructed from a smaller guage
> >*>sheet. Not sure what guage it is but it's pretty thin.
> >*>
> >*>Walker
> >*>
> >*>_______________________________________________
> >*>Manage membership or unsubscribe at:
> >*>>*>http://mailman.qth.net/mailman/listinfo/theforge
> >*>theforge
> >*>mail list group photo site is http://www.photoaccess.com
> >*>Login: blacksmithblacksmith at hotmail.com
> >*>password: anvil
> >*>___________
> >*>
> >*>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list