[TheForge] patina on aluminium?
Doug Ayen
ayen at homeport.org
Thu Sep 15 14:54:18 EDT 2005
Thus Spake S. Pohlman (ajarrod at voyager.net):
> I have some old 4X4 wheels. In good shape but the finish is gone. Is
> there a way to color them ? could they be cold blued like a gun barrel?
>
> Stu
Adonizing is the way to go if you want a bright color.
If you're OK with black, there's a cold black patina available for
aluminum. Brownells carries it. Don't know how durable it is, though.
--doug