[TheForge] Cookie cutter type of press blade

Chris Worsley worsley at verizon.net
Tue Sep 13 06:30:01 EDT 2005


I should think that you would save time and money - time is money - if 
you found a laser cutter guy that you could fax your patterns to and 
have him cut your pieces. Depending on how many you have cut, this is 
getting more affordable.
A friend now does this for steel parts and finds it quite cost 
effective. I don't know who he uses, but if you are interested I can 
find out.
 
Chris

Jerry Smith wrote:

>I need to made a cookie cutter type of cutting or
>press blade to cut thin aluminum in stacks. I was
>thinking of using old hacksaw blades, form the shape
>and then sharpen the edges.
>
>Anyone do anything like this?
>
>Jerry
>  
>





More information about the TheForge mailing list