[TheForge] Welding Copper ?
Grant Marcoux
gblacksmith at alamedanet.net
Thu Sep 8 17:40:11 EDT 2005
Rick: Pete is right re the steel wool fragments. Try scotch brite....I use
purple for non ferrous. Grant
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net]On Behalf Of Peter Fels And
Phoebe Palmer
Sent: Wednesday, September 07, 2005 10:52 PM
To: Sponsored by ABANA
Subject: Re: [TheForge] Welding Copper ?
Rick;
Watch out for steel wool for this for 2 reasons..
1 it often comes with an oil based rust inhibitor which will mess
with the solder wetting the copper...and
2. It will leave tiny steel fragments which can rust and mess
with the patina that forms....PF
Rick wrote:
> Hey guys -
>
> Thanks for all the replys about welding copper. I will probably go
> with brazing when I get some rod, but for a try out I soldered a leaf
> to a vine and a tendril of different size wires. The leaf is made out
> of copper roof flashing and is quite thin. I took steel wool over it
> to clean it before I shaped it, then after all was done, I clear coated
> it. (My wife likes the look of copper and she gets most of my tryouts.)
>
> I put 3 pictures of it in the "current works" folder on the Photo
> Access site listed at the bottom of all our emails. Feel free to
> comment on it, my feelings won't be hurt as this is just a tryout and
> since it worked, what else could I ask for?
>
>
> Yours,
> Rick Crawford at Rafter Lazy C
> Home of Smoky Forge and Lem the Wonder Mule
> In the middle of Northern Illinois
>
> http://www.smokyforge.com
> rick at smokyforge.com
>
>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
--
No virus found in this incoming message.
Checked by AVG Anti-Virus.
Version: 7.0.344 / Virus Database: 267.10.19/93 - Release Date: 9/8/2005
More information about the TheForge
mailing list