[TheForge] Welding Copper ?

Roy Wilson rwilson9 at twcny.rr.com
Mon Sep 5 17:58:17 EDT 2005


  
======= On 2005-09-05, at 17:06:20 Rick wrote: =======

>Hi all you guys and gals -
>
>    I have just decided on copper for the material of choice on a project 
>involving grape leaves and vines.  However, I have never welded copper and 
>am not sure if or how it is possible.  Please fill me in and help me learn 
>on this project as I go.
>
>    By the way, I only have a 120V Lincoln mig welder or oxy-acetylene or 
>stick welder.  Nothing else, (like tig which I think would be easiest to 
>try).

	Torches work fine, although my brazing torch is just acetylene.  #14 Romex-type house wire works just fine as rod, and you can usually get 14 or 12 already bare as grounding line anyplace that sells electrical supplies.


"Caesar si viveret, ad remum dareris." - Xanthippos

Roy Wilson - rwilson9 at twcny.rr.com
2005-09-05



More information about the TheForge mailing list