[TheForge] andiron bar replacement

PlumDon at aol.com PlumDon at aol.com
Sun Oct 23 20:29:28 EDT 2005


 
That's really pricey, Jim. I have some inconel studs holding the insulation  
to my forge door and they do hold up well, even in that heat. I just mig 
welded  them to the inside of the door. Is it harder to weld in large sizes? 
 
I dont know what a 3/4" square x 3' bar of stainless would cost but  methinks 
cheaper. 
 
In a message dated 10/23/2005 7:26:45 PM Eastern Standard Time,  
jbin at well.com writes:

Inconel  625 will last a lot longer (probably forever) but is somewhat  
pricey  (3/4" dia bar 3' long is 189.00) and difficult to weld

On Oct 23, 2005,  at 10:18 AM, PlumDon at aol.com wrote:

> I have a customer who burns  out their andiron bars in a year. She  
> has  asked me to use  wrought iron this time as she thinks it might last  
>  longer.  Any  one have any suggestions for a more durable  material or 
approach?
>


 