[TheForge] Re: andiron bar replacement
Mike Spencer
mspencer at tallships.ca
Sun Oct 23 15:42:59 EDT 2005
> I have a customer who burns out their andiron bars in a year.
Weld on rails from stainless round. Sleeve square HSS over the SS.
Replace the sleeves annually or as needed, minimal work for a
small maintainance fee.
Not that I've ever done that, of course. YMMV etc. etc. :-)