[TheForge] toys how many?
Dan Scheid
Damales at earthlink.net
Tue Oct 18 02:23:28 EDT 2005
I guess the question is should I?
Is it worth the time and space/money
Dan
I'm not sure I understand the question Dan. Aren't you going to make a set
of rolls as an accessory to the hyd press?
Frosty
------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks
Meadow Lakes, AK.
From: "Dan Scheid" <Damales at earthlink.net>
>
> In a few months I will be moving so the shop building talk has been great.
> The Phase you can never have too many tools fits me. But I do want to be
> logical with the move and the expansion. I have a good air hammer and I am
> going to build a hydraulic press. The question is a rolling mill is it
> worth
> the time and space if you have both a press and a hammer? I've had 5
> accounts wanting Damascus taken very thin .04" so I can see using it there
> but then again you can get Very even with a press. Input....ideas?
> Dan Scheid
>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list