[TheForge] Re: Air hammer anvil height

Peter Fels And Phoebe Palmer artgawk at thegrid.net
Tue Oct 18 00:16:01 EDT 2005


Is it reasonable to suppose that the smaller the hammer, the 
higher the dies?.......Pete F

Mike Spencer wrote:
>>I haven't used it yet so don't really know from experience what a
>>comfortable height from the ground to the work should be.
> 
> 
> FWIW, my 25# Jardine was on the floor in the old shop.  Now I have  up
> on 8" blocks and I like it way better.  If I were to do it over, I
> *might* even go a bit higher.  Dunno how manyinches.  I'll check whem
> I next go out to the shop.
> 
> - Mike
> 