[TheForge] toys how many?
Dan Scheid
Damales at earthlink.net
Mon Oct 17 13:52:10 EDT 2005
In a few months I will be moving so the shop building talk has been great.
The Phase you can never have too many tools fits me. But I do want to be
logical with the move and the expansion. I have a good air hammer and I am
going to build a hydraulic press. The question is a rolling mill is it worth
the time and space if you have both a press and a hammer? I've had 5
accounts wanting Damascus taken very thin .04" so I can see using it there
but then again you can get Very even with a press. Input....ideas?
Dan Scheid