[TheForge] Mystery Metal
Jonathan Nedbor
jonned at hvc.rr.com
Thu Oct 6 14:24:29 EDT 2005
So, I suppose my mystery metal is actually stainless steel. I was able to
run a nice fused bead with my tig welder. As I understand it MONEL does not
weld. Is that correct?
The only thing I am surprised by is the "oxide" on the surface of the bars,
brownish. NOt what I would expect from Stainless. Also, I sanded the
surfaces of the 2 small pieces and the area near the weld turned a light
brown, with no hint of blue or grey.
There is a number stamped near one end, 4316. Does that indicate anything to
any of you?