With conventional (commercially used) drop hammers, the "bounce" is a
real advantage, as it becomes the start of the next stroke, i.e., the
bounce in essence overcomes the inertia and provides the start of the
lift of the die to it's "up" position for the next blow, thereby
greatly easing the workload of the lift mechanism.
Michael
-----Original Message-----
From: Bruce Freeman <FREEMAB at pt.fdah.com>
To: theforge at mailman.qth.net
Sent: Wed, 05 Oct 2005 08:07:49 -0400
Subject: [TheForge] "DROP" Hammer - Question
I've been wondering for some time about that idea - loose lead fill in
a hollow
hammer. Seems to me that only would only work in a "driven" (e.g.,
hand-held
dead-blow) hammer.
I would gusss that, in a drop hammer, everything (hammer and lead fill)
would be
falling at the same speed. Unless compression of the fill were
involved, there
would be no less tendency to bounce. But then, I've never tried it.
Bruce
NJ
>>> lughaid at earthlink.net 10/4/2005 4:20:09 PM >>>
Yup, I used to work with Michael Stewart at Quick Silver Minting,
Tool and Die. We made the crank up drop hammer you saw, and quite a
few others. Hammer head is a well casing with a 3 inch plate welded
to the base, capped and filled with lead shot. about 125 pounds head
weight for a dead drop to keep from double striking the
"coins".
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list