On Oct 31, 2005, at 4:59 AM, Bruce Freeman wrote:

> I do vaguely remember his discussion about "packing the edge" of a  
> knife.  Pure nonsense.

I thought the metallurgical effect of "packing" was to reduce grain  
size.