[TheForge] Fountain Spout
debmiller at fuse.net
debmiller at fuse.net
Thu Nov 10 07:43:01 EST 2005
Brass or cast iron, depending on size of the opening. I would recommend brass.
There are plenty of online fountain parts suppliers for guidence. I have also used stainless of course, but not for an "old" look.
Ray
Cincinnati
---- ductility at juno.com wrote:
> I have a client that wants a spout for a fountain. Very simple project
> but with one problem, what to make it out of? Seeing it is a outside
> fountain the water will have chemicals in it and could corrode the wrong
> type of metal. Anybody out there ever dealt with this problem and what
> is the solution. The finish has to be old, antique, maybe like rusted
> iron with the deep dark brown look.
>
> Thanks,
> Jeff in Phoenix
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
More information about the TheForge
mailing list