[TheForge] hot portable atmospheric forges may need propylene
Keporter at aol.com
Keporter at aol.com
Tue May 31 20:39:02 EDT 2005
In a message dated 5/31/2005 5:23:58 P.M. Pacific Standard Time,
robi5515 at bellsouth.net writes:
Right I was trying to say that the O2 is limited by the Hi % of Nitrogen in
the air.
You are also are heating and exhausting the nitrogen so you are loosing
potential heat.
The Propylene sounds interesting.
I might try swapping a 11/4" "T-Rex" AB for my blown burner in my vertical
pipe forge.
If the burner is located at least 10" below the billet door opening, it is
way more efficient than a horizontal pipe forge.
Chuck
Chuck
Especially important tasks deserve particular tool designs dedicated to
doing them best. The tube forge is a general light duty portable forge, and will
always be beaten by specialty forges at specialty tasks.
Mike P.