I'm using a Sandia Forge (intake preheaters) and at about 9 psi of propane,
I can get to a nice welding heat. I haven't actually verified the
temperature, but assuming normal A36 steel Im in the 2600 to 2800 degree
range. Normally aspirated.
mike
At 11:37 AM 5/30/2005, you wrote:
>On Monday, May 30, 2005, at 08:17 AM, Chuck Robinson wrote:
>
>>I'd like to hear from anyone who uses an atmospheric propane burner of
>>any design that actually has accurately measured a forge temperature
>>hotter than 2500 F-
>>with out usig auxilliary O2, compresser air or a blower boost.
>>Chuck
>
>
> Mike Linn
> Artist Blacksmith
> McCalla, AL
> AFC Webmaster
>http://afc.abana-chapter.com
>
>______________________________________________________________________
>
>"Many of life's failures are people who did not realize how
> close they were to success when they gave up. "
> ~ Thomas A. Edison
>______________________________________________________________________
>
>
>
>
More information about the TheForge
mailing list