Dang de doodle, but I do like talking with you guys. Now, according to my
research (book two) it shouldn't be possible to upset weld titanium at all. Ti
is supposed to form oxides way too fast under heat to be welded any way but
by fusion (electric arc) or within special inert atmospheric brazing ovens.
What this means to me is that somebody has come up with a better flux. If
someone has come up with a flux that makes this possible, it should also work for
brazing titanium, which is my interest. What flux is it?