Acetone and compressed!  Got'em both..Thanks...I'll try it in the morning.

Let ya know results on Sunday!

Daniel Kretchmar
www.irontreeworks.com

Isn't sanity really just a one trick pony, anyway? I mean, all you get is one
trick, rational thinking! But when you're good and crazy
ooh hoo hoo hoo
the
sky's the limit!
The Tick


Quoting Ron Childers <munlaw2 at hcsmail.com>:

> Also blow with compressed air after soaking. Ron C
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Darrell
> Sent: Wednesday, May 18, 2005 2:54 PM
> To: Sponsored by ABANA
> Subject: Re: [TheForge] hot head torch advice
>
> If it is like mine, the tip of the torch unscrews and there is a part with a
> very small orifice. That is what is plugged. Acetone should clean it. The
> tank side has a brass filter.
>
> Darrell
>
> ----- Original Message -----
> From: "Daniel Kretchmar" <irontree at visi.com>
> To: "Sponsored by ABANA" <theforge at mailman.qth.net>
> Sent: Wednesday, May 18, 2005 11:08 AM
> Subject: [TheForge] hot head torch advice
>
>
> > Hey All,
> >     My wife has a hot head torch for map gas (like a little single gas
> propane
> > torch) for lamnpwork (glass beads) but she left the Map gas tank on it's
> side
> > and some of the "oil" (poly-something or other) leaked into the torch and
> now
> > the thing won't light...No gas comes out, though it will come out of the
> tank
> > without the hose on, so it's not empty.  The stuff is in the hose and the
> head.
> >
> > When I tried a new hose, it didn't help
> >
> > Any ideas how to clear the torch.?
> >
> >
> > Daniel Kretchmar
> > www.irontreeworks.com
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
>



More information about the TheForge mailing list