FWIW

I went and looked at several (5) MSDS's for boiled linseed oil on the 
net and not one of them listed any other ingredients other than 
linseed oil , no driers or solvents, nada. None of the MSDS listed 
any severe health hazards

>"Symptoms of Overexposure................	INHALATION: NONE 
>EXPECTED. SEVERE OVEREXPOSURE MAY CAUSE COUGH AND IRRITATION OF 
>RESPIRATORY TRACT. INGESTION: INEDIBLE - NOT BE TAKEN INTERNALLY. 
>MAY CAUSE NAUSEA, VOMITING & DIARRHEA. SKIN CONTACT: NONE EXPECTED. 
>EYE CONTACT: MAY CAUSE IRRITATION. "

and lots of info about fire danger. So I kind of wonder about the 
source of information that was used for that article...
-- 
Jim Binnion

James Binnion Metal Arts
Phone (360) 756-6550
Toll Free (877) 408 7287
Fax (360) 756-2160
http://www.mokume-gane.com
jbin at mokume-gane.com
Member of the Better Business Bureau


More information about the TheForge mailing list