[TheForge] A recipe for Emperor Wilson...
Roy Wilson
rwilson9 at twcny.rr.com
Tue Jun 14 14:53:11 EDT 2005
======= On 2005-06-14, at 13:55:47 Phlip wrote: =======
>
>... who is finally speaking to us again...
Sorry, been busy. You know how it is, things to see, people to do...<G>
Seriously, I've been busy enjoying better health and once again being single.
>Source for Recipe Presented
>De Honesta Voluptate by Platina, 1475 - Redaction by Cariadoc
Hmm... a recipe presented by "The Gilded Truthful Admirer of Voluptuousness"? I see why it needed redaction.<G>
>Just in case any fell off your wagon recently ;-)
Hey, I didn't just fall off the turnip wagon! Those bruises have been gone almost a week!<G>
So what have you been making of late, Lady Phlip? BTW, I love the period sunglasses in that pic of you and John...<G>
I fired up the coal forge about a week ago to beat a machete out of a chunk of old leaf spring. The brush in my sidelot had grown up so much even the powered reel on the brush hog couldn't knock it down.
Tips on lighting up a coal forge that's been dormant over 2 years in upstate NY:
1) Make SURE you've chased out ALL the skunks that took up residence in the pedastal box.
2) Raccoons find the chimney and flue of forges to be excellent breeding creches.
3) Water left in covered quench buckets for more than a year gets STOLEN!
<G>
= = = = = = = = = = = = = = = = = = = =
Emperor Wilson
WINS#6
"Caesar si viveret, ad remum dareris." - Xanthippos