[TheForge] Re: brill dit stock (grrr)
Justin Fellenz
sunironworks at yahoo.com
Thu Jun 2 10:55:33 EDT 2005
It's an 8mm bold with about a 6mm extractor in it now. I tried the
dremel approach to dish it out to get a good center punch. Messed up
the top 1/16" of the hole, no big deal. Hope play-doh holds the acid...
J
--- Ron Childers <munlaw2 at hcsmail.com> wrote:
> Justin,
>
> If all else fails, you should be able to grind the screw extractor
> out with
> a Dremmel Tool. If you mess up the threads, you can repair with a
> Helicoil
> or Keensert, etc. How big is the bolt?
>
> Ron Childers
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list