Nah, I'd rather start with a piece of 1/4" flat plate...
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Darrell
Sent: Friday, July 29, 2005 3:39 PM
To: munlaw2 at hcsmail.com; Sponsored by ABANA
Subject: Re: [TheForge] Putting new handles on old skillets
You could make a handle out of iron, weld it to the pan with nickel rod.
Then using some more nickel rod weld some kind of pattern on the handle and
grind it all smooth so the weld doesn't show because it will look like part
of the pattern.
Darrell
-----