[TheForge] Putting new handles on old skillets

Darrell darrell at machinemaster.com
Fri Jul 29 15:39:28 EDT 2005


You could make a handle out of iron, weld it to the pan with nickel rod.
Then using some more nickel rod weld some kind of pattern on the handle and
grind it all smooth so the weld doesn't show because it will look like part
of the pattern.

Darrell

----- Original Message ----- 
From: "Ron Childers" <munlaw2 at hcsmail.com>
To: "'Sponsored by ABANA'" <theforge at mailman.qth.net>
Sent: Friday, July 29, 2005 12:24 PM
Subject: RE: [TheForge] Putting new handles on old skillets


> Good shot; that's heresy, but I was trying to be nice to the poor
misguided
> soul...
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Justin Fellenz
> Sent: Friday, July 29, 2005 1:53 PM
> To: Sponsored by ABANA
> Subject: Re: [TheForge] Putting neu handles on old skillets
>
> :<grin>:
>
> --- Dan Tull <dantull at numail.org> wrote:
>
> > Wood?????????
> > We're blacksmiths!
> >
> > ----- Original Message ----- 
> > From: "Justin Fellenz" <sunironworks at yahoo.com>
> > To: "Sponsored by ABANA" <theforge at mailman.qth.net>
> > Sent: Friday, July 29, 2005 11:54 AM
> > Subject: RE: [TheForge] Putting neu handles on old skillets
> >
> >
> > Is there enough meat in the handle stub to drill and tap for a
> > throughbolt to hold on a nice wooden handle?
> >
> > JRF
> >
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>



More information about the TheForge mailing list