[TheForge] Seasoning tasting spoons

Bruce Freeman FREEMAB at pt.fdah.com
Fri Jul 29 11:13:07 EDT 2005


Are you sure that was a tempering color?  Granted, that's about the right color for the temperature (considering the inaccuracy of oven controls).  However, I expect you were seeing the color due to the oil.

BTW.  Crisco is not the best choice for this.  Polyunsaturated vegetable oil is better.

Bruce
NJ

>>> dski1045 at qis.net 7/29/2005 9:48:55 AM >>>
Phlip,

I recently made some table ware for use at Ren-faire events.  I seasoned
them  in the oven at 375 with Crisco (like I do cast iron frypans etc).  I
found that I should have done one cycle without the Crisco in order to first
get an even color over the entire utensil.  At 375 (according to oven
setting), the utensils picked up a very nice gold/bronze tempering color.
But where the Crisco puddled, such as in the bowls of the spoons, or
wherever a part of the utensil rested on the cookie tray, the color did not
take.

Also, next time, I will season with spoons facing down for the first cycle
using the Crisco.  I did a total of 3 cycles with Crisco.

Since you may have more experience from a cooks perspective:  how low a
temperature can one use for seasoning cookware?  I have seen temperatures in
the 350 to 425 referenced.  My customer was pleased with the bronze color,
but I am wondering if I would get effective  seasoning of the utensil at a
low enough temperature so as not to get a temper color on the steel, i.e.
keep the bright steel color.

D-ski
Westminster, MD

----- Original Message ----- 
From: "Phlip" <phlip at 99main.com>
To: <theforge at mailman.qth.net>
Sent: Thursday, July 28, 2005 8:15 AM
Subject: [TheForge] Pineapple twist


>
> Can someone run over the instructions for the Pineapple Twist for me? I
have
> a project that it would be very appropriate for (actually a couple) and
I'd
> like to get it right ;-)
>
> As the project is making a couple of steel tasting spoons for a couple of
> friends, would I be OK seasoning the spoons as I normally would a cast
oron
> frying pan, or a steel wok? Or is there another finish that you guys would
> suggest?
>
> Saint Phlip,
> CoD
>
> "When in doubt, heat it up and hit it with a hammer."
>  Blacksmith's credo.
>
>  If it walks like a duck, and quacks like a duck, it is probably not a
> cat.
>
> Never a horse that cain't be rode,
> And never a rider who cain't be throwed....
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge 
> theforge mail list group photo site is
> http://www.photoaccess.com 
> Login:  blacksmithblacksmith at hotmail.com 
> password:  anvil
> ___________
>
>
>


_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge 
theforge mail list group photo site is
http://www.photoaccess.com 
Login:  blacksmithblacksmith at hotmail.com 
password:  anvil
___________





More information about the TheForge mailing list