[TheForge] Pineapple twist

Ron Childers munlaw2 at hcsmail.com
Thu Jul 28 10:15:39 EDT 2005


Phillip,

For step-by-step instructions on pineapple twists go to anvilfire.com, click
on "Navigate Anvilfire", click on iForge, & scroll down to # 11, The
illustrations are easy to follow.

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Ron Childers
Sent: Thursday, July 28, 2005 9:25 AM
To: 'Sponsored by ABANA'
Subject: RE: [TheForge] Pineapple twist

PT's are easy; just chisel (or incise) grooves on all 4 sides- make 'em
even- heat and twist right at least 1 full turn. (Do it right the first
time)Heat & re square the bar. Incise again and twist left 1/2 turn (take
care of what's left). For a smoother grip you may want to forge a slight
radius on the corners. The more you twist, the smaller the diamonds.
Experiment (:

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Phlip
Sent: Thursday, July 28, 2005 8:16 AM
To: theforge at mailman.qth.net
Subject: [TheForge] Pineapple twist


Can someone run over the instructions for the Pineapple Twist for me? I have
a project that it would be very appropriate for (actually a couple) and I'd
like to get it right ;-)

As the project is making a couple of steel tasting spoons for a couple of
friends, would I be OK seasoning the spoons as I normally would a cast oron
frying pan, or a steel wok? Or is there another finish that you guys would
suggest?

Saint Phlip,
CoD

"When in doubt, heat it up and hit it with a hammer."
 Blacksmith's credo.

 If it walks like a duck, and quacks like a duck, it is probably not a
cat.

Never a horse that cain't be rode,
And never a rider who cain't be throwed....

_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________



_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________






More information about the TheForge mailing list