-------------- Original message --------------
> Dan,
> I think you may be wasting your time making balls for the Whisper Mama.
> What makes the balls work is to have the flame coming up through the balls
> so the balls absorb the heat.
> With the Whisper Mama, the top layer of balls will get hot but the ones
> below that layer will be insulated from the flame.
>
> Darrell
So far as using thermal mass efficiently, your point is well made. Unfortunately, over a period of time the entire mass will heat pretty close to flame temperature through conduction, at which point it is likely to start destroying the ceramic fiber insulation.
Mike P.
>
>
> >> >
> >
> >
> >
> >
>
>
>
>