> (I don't know where we'd come up with ceramic chips, > otherwise.) BTW, Flamefast (UK) sells ceramic chips, which are used in their forges, by the bag. However, I wouldn't waste the money when you can make nice round refractory balls out of high temp castable (or rammable) refractory. Mike P.